AMS-T-21014 Class 2 applications for tungsten alloy rod:These kinds of rods could be machined further, which are usually used to making the parts of counterweight,AMS-T-21014 Class 2 radiation shielding, military defense appliance, welding rod, AMS-T-21014 extrusion die, also for some sports fields, such as darts, billets, golf club, etc. Besides, we can manufacture and offer tungsten alloy rod as the counterpart of Anviloy 1150, whose properties are much similar.
AMS-T-21014 Class 2 Tungsten Alloy Product Description
Diameter: 2.0-100.0mm
Length: 50-1000mm
Density: 15.8-18.75 g/cm3
Composition: W content: 85-99%, W-Ni-Fe, W-Ni-Cu
AMS-T-21014 Class 2 Tungsten Alloy Surface: Sintering surface, Forged surface, Ground surface
AMS-T-21014 Class 2 Tungsten Alloy Advantages
High density(17.0-18.5g/cm3).
Good machinability
Good mechanical properties.
High modulus of elasticity
High absorption capacity against x-rays and γ-rays
Harmless to the health and environments.
AMS-T-21014 |
Class 2 |
Class 2 |
Composition |
92W5Ni3Fe |
93W4Ni3Fe |
Density (g/cm3) |
17.50±0.15 |
17.60±0.15 |
Heat Treatment |
Sintering |
Sintering |
Tensile Strength (MPa) |
900-1100 |
900-1100 |
Elongation (%) |
16-26 |
16-24 |
Hardness(HRC) |
25-29 |
26-30 |
AMS-T-21014 |
Class 2 |
(AMS 7725C) |
- |
ASTM-B-777-99 |
Class 2 |
Density Gms/cc |
17.5 |
Hardness Rockwell C |
26 |
Ultimate Tensile |
114,000 |
Yield Strength |
84,000 |
Elongation (% in 1″) |
7 |
Proportional Elastic |
46,000 |
Modules of |
47 x 10^6 |
Coefficient of Thermal |
4.62 |
Thermal Conductivity |
.20 |
Electrical Conductivity |
13 |
Magnetic Properties |
Slightly Magnetic |
17.6 (92.5%W, Balance Ni Fe) |
|
AMS-T-21014 |
Dimetal |
(AMS 7725C) |
- |
ASTM-B-777-99 |
- |
Density Gms/cc |
17.6 |
Hardness Rockwell C |
30 |
Ultimate Tensile |
120,000 |
Yield Strength |
90,000 |
Elongation (% in 1″) |
4 |
Proportional Elastic |
55,000 |
Modules of |
52 x 106 |
Coefficient of Thermal |
4.5 |
Thermal Conductivity |
.27 |
Electrical Conductivity |
14 |
Magnetic Properties |
Slightly Magnetic |
17.7 (93%W, Balance Ni Fe) |
|
AMS-T-21014 |
Super Chatter Free |
(AMS 7725C) |
- |
ASTM-B-777-99 |
- |
Density Gms/cc |
17.7 |
Hardness Rockwell C |
32 |
Ultimate Tensile |
125,000 |
Yield Strength |
95,000 |
Elongation (% in 1″) |
4 |
Proportional Elastic |
60,000 |
Modules of |
53 x 10^6 |
Coefficient of Thermal |
4.5 |
Thermal Conductivity |
.27 |
Electrical Conductivity |
14 |
Magnetic Properties |
Slightly Magnetic |
18 (95%W, 3.5%Ni, 1.5%Cu) |
As a AMS-T-21014 Class 2 Tungsten Alloy manufacturer, we usually keep hundreds tons AMS-T-21014 Class 2 Tungsten Alloy in stock each month. Based on these stock source, our advantage has spread into steel process like : cutting ( any size and any shape ) drilling, welding, milling, welding. We can also provide the AMS-T-21014 Class 2 Tungsten Alloy in machining parts and steel structure.
TEL : 0086-18317160019
E-mail : [email protected]
Address : No.230,1st Floor,Building No.1,No.221 Of Huashen Road,Free Trade Area Of Pudong New District,Shanghai China