The chemical elements and property make ABS AH36 steel plate have a lot of features
First, ABS AH36 steel plate has good toughness. In order to ensure the quality and toughness, the
chemical composition of Mn/C is required to be more than 2.5, and the carbon equivalent of ABS AH36 steel plate is also strictly required.
Besides, ABS AH36 steel plate has good strength, corrosion resistance, weldability, processing performance and surface quality. So that it can adapt to the harsh working environment on the sea.
In addition, ABS AH36 steel plate should be produced by steel mills approved by the ABS inspection department
ABS AH36 steel plate chemical elements
Grade | C max | Si max | Mn | P max | S max | Als min | Ti max | Cu max | Cr max | Ni max | Mo max | Nb | V |
ABS AH36 | 0.18 | 0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 | 0.02-0.05 | 0.05-0.10 |
Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.36% (thickness ≤ 50mm),≤0.38%( when the thickness > 50-100).
Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.
ABS AH36 steel plate strength and property
Grade | Rm (MPa) | Re(MPa) min | A% min | Akv/J min | ||||||
E.T °C | Thickness (mm) | |||||||||
≤ 50 | > 50-70 | > 70-100 | ||||||||
L | C | L | C | L | C | |||||
ABS AH36 | 490-630 | 355 | 21 | 0 | 34 | 24 | 41 | 27 | 50 | 34 |
ABS AH36 steelABS AH36 steel plate is mainly used to build hull structure and need to work in sea water at most times. The harsh work environment give a lot of high requirements to ABS AH36 steel plates. welcome to contact katalor if you are looking for the supplier of ABS AH36 steel plate.