Quality |
S275JR(Fe430B) |
According to standard |
EN10025-2:2004 |
Number |
1.0044 |
EN10025 S275JR steel plate Chemical composition:
C% (max) |
Si% |
Mn% (max) |
P% (max) |
S% (max) |
N%(max) |
Cu%(max) |
|
0,21 |
- |
1,50 |
0,035 |
0,035 |
0,012 |
0,040 |
Cast analysis |
0,24 |
- |
1,60 |
0,045 |
0,045 |
0,014 |
0,045 |
Product analysis |
EN10025 S275JR steel plate Metod of deoxidation FN rimming steel not permitted
maximum 0.22 ladle analysis, max 0.25 product analysis for thickness over 40 mm to 100 mm
for nominal thickness > 100 mm the C content by agreement
the max value does not apply if the chemical composition shows a minimum total Al content of 0.020%
the max value does not apply if the chemical composition shows a minimum total Al content of 0.015%
EN10025 S275JR steel plate Temperature °C
S275JR’s Equivalent material including Fe 430 B ,Q255A,St 44-2,E 28-2,43 B and St4kp-2. Katalor is the supplier of EN10025 S275JR steel plate , any question for EN10025 S275JR steel plate is welcomed to send to katalor.